J. Eng. Mater. Technol. July 2011, 133(3): 031002.
Published Online: June 24, 2011
...L. G. Zhao Finite element analyses of oxygen diffusion at the grain level have been carried out for a polycrystalline nickel-based superalloy, aiming to quantify the oxidation damage under surface oxidation conditions at high temperature. Grain microstructures were considered explicitly...
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. July 2011, 133(3): 031001.
Published Online: June 23, 2011
...Z. J. Moore; R. W. Neu Fatigue life modeling of anisotropic materials such as directionally-solidified (DS) and single-crystal Ni-base superalloys is often complicated by the presence of notches coupled with dwells at elevated temperatures. This paper focuses on an approach for predicting low cycle...
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. April 2011, 133(2): 021023.
Published Online: March 23, 2011
... blades with the absence of such data. This paper describes innovative methods used to predict high-temperature fatigue of IN738LC, a dual-phase Ni-base superalloy. Three sets of experimental data at different temperatures are used to evaluate and examine the validity of extrapolation methods...
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. April 2011, 133(2): 021013.
Published Online: March 21, 2011
...Calvin M. Stewart; Ali P. Gordon; Erik A. Hogan; Ashok Saxena Creep deformation and rupture experiments are conducted on samples of the Ni-base superalloy directionally solidified GTD-111 tested at temperatures between 649 ° C and 982 ° C and two orientations (longitudinally and transversely...
Journal Articles
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. July 2010, 132(3): 031005.
Published Online: June 16, 2010
...S. Chiozzi; V. Dattoma; F. Panella This work concerns single crystal Ni-based superalloy welded through the capacitor discharge welding (CDW) process. The static and fatigue behavior of CMSX-4 type single crystal alloy has been analyzed, performing mechanical tests on square specimens in order...
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. January 2010, 132(1): 011001.
Published Online: November 2, 2009
... with that of Alloy 617, indicating its slower crack-growth rate. Fractographic evaluation of the broken specimen surface revealed combined fatigue and ductile failures. cracks ductility fatigue fractography nickel alloys superalloys crack-growth rate cyclic loading temperature load ratio...
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. July 2009, 131(3): 031008.
Published Online: May 26, 2009
... superalloy IN100. The model incorporates the dominant creep deformation mechanism, coupling between the creep and plasticity models, and effects of prior plastic strain. The initial room temperature residual stress and plastic strain profiles provide the initial conditions for relaxation predictions using...
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. July 2008, 130(3): 031010.
Published Online: June 11, 2008
...Duyi Ye; Jinyang Zheng In this paper, both the dissipation of the plastic-strain energy and the exhaustion of the static toughness during high-temperature low-cycle fatigue of GH4145/SQ superalloy were investigated. Together with the analysis of the microscopic aspects of the material, an energy...
Journal Articles
Journal Articles
Journal Articles
Publisher: ASME
Article Type: Technical Papers
J. Eng. Mater. Technol. January 2005, 127(1): 23–32.
Published Online: February 22, 2005
... of anisotropic material behavior and the effect of changes in grain orientation as the crack grows. The effect of local crystallography was studied in multicrystalline Compact-Tension (CT) specimens of pure nickel and a cast Ni-based superalloy. Orientation Imaging Microscopy (OIM) was used to map...
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. January 2005, 127(1): 119–129.
Published Online: February 22, 2005
...G. Bande; J. A. Nemes A new approach used for single crystal (SC) materials analysis is described. Its principle is based on the extension of predictive models for isotropic material behavior to anisotropic materials such as SC nickel base superalloys. A viscoplastic model describes the material...
Journal Articles
Publisher: ASME
Article Type: Research Papers
J. Eng. Mater. Technol. July 2005, 127(3): 325–336.
Published Online: February 2, 2005
...M. M. Shenoy; A. P. Gordon; D. L. McDowell; R. W. Neu A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times...
Journal Articles
Publisher: ASME
Article Type: Technical Papers
J. Eng. Mater. Technol. April 2004, 126(2): 204–212.
Published Online: March 18, 2004
...Rong Liu; Matthew X. Yao; Xijia Wu Two cobalt-based superalloys containing 1.6% and 2% carbon respectively were studied, with the emphasis on the influence of the carbon content on their microstructures, wear resistance, and mechanical properties. Phase formation and transformation...
Journal Articles
Publisher: ASME
Article Type: Technical Papers
J. Eng. Mater. Technol. April 2002, 124(2): 103–111.
Published Online: March 26, 2002
... superalloy developed for gas turbine applications. Ziebs et al. 17 have carried out an extensive investigation on this nickel-base alloy behavior at 850 ° C (CSR tensile tests (tension positive), creep, relaxation, one-dimensional and biaxial cyclic...
Journal Articles
Publisher: ASME
Article Type: Technical Papers
J. Eng. Mater. Technol. July 2001, 123(3): 349–354.
Published Online: February 28, 2001
... alloys nickel alloys superalloys molybdenum alloys finite element analysis 01 February 2000 28 February 2001 Contributed by the Materials Division for publication in the JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY . Manuscript received by the Materials Division February 1...
Journal Articles
Publisher: ASME
Article Type: Technical Papers
J. Eng. Mater. Technol. July 2000, 122(3): 300–304.
Published Online: March 13, 2000
...D. J. Arrell; J. Bressers; J. Timm Thermo-mechanical fatigue of nickel-base superalloys has been carried out for more than twenty years, but a unified standard for such tests has yet to be fully formulated. As a consequence of this, even excluding differences in testing procedure from laboratory...
Journal Articles
Publisher: ASME
Article Type: Technical Papers
J. Eng. Mater. Technol. July 2000, 122(3): 315–320.
Published Online: March 1, 2000
...] nickel alloys chromium alloys cobalt alloys superalloys fatigue slip creep fracture voids (solid) scanning electron microscopy modelling With increasing use of long-term operated gas turbine power plants, it becomes important to improve the accuracy of creep-fatigue life prediction...